Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Limiting Pressure Velocity = 0.666 MPa-m/sec Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.666 MPa-m/sec
19000 psi-ft/min
100 fpm
Techmer ES Luriblend® PA6/6 GF30 TS1 BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R..
Limiting Pressure Velocity 0.666 MPa-m/sec
19000 psi-ft/min
100 fpm
Techmer ES Luriblend® PA6/6 GF30 TS15 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R..
Limiting Pressure Velocity 0.666 MPa-m/sec
19000 psi-ft/min
100 fpm
Techmer ES Luriblend® PA6/6 GF33 TS15 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R..
Limiting Pressure Velocity 0.666 MPa-m/sec
19000 psi-ft/min
100 fpm
Techmer ES Luriblend® PA6/6 GF33 TS15 BK 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R..
Copyright © lookpolymers.com All Rights Reserved