Polymer Property : Limiting Pressure Velocity = 10.7 psi-ft/min Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.000376 - 0.000409 MPa-m/sec
10.7 - 11.7 psi-ft/min
3 m/min
Polikim EFALON® T-100 Virgin PTFE
Applications: Gaskets, seals, O-rings, V-Rings, compression packings and similar sealing parts, Bushes, bearings and piston rings, Electrical insulators, Sliding supports, Conveyor belts, Coated tu..