Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 1.33 MPa-m/sec | 38000 psi-ft/min | at 0.127 m/s |
Cast Nylons Nycast® Nyloil®-FG Lubricated Nylon, Food Grade NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |
|||
Limiting Pressure Velocity | 1.33 MPa-m/sec | 38000 psi-ft/min | at 0.127 m/s |
Cast Nylons Nycast® Nyloil® Lubricated Nylon NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |
|||
Limiting Pressure Velocity | 1.33 MPa-m/sec | 38000 psi-ft/min | at 0.127 m/s |
Cast Nylons Nycast® Nyloil®-MDX Lubricated Nylon, MoS2 Filled NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |