Polymer Property : Limiting Pressure Velocity = 0.330 MPa-m/sec Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.330 MPa-m/sec
9420 psi-ft/min
at 0.1 m/s unlubricated
Quadrant EPP Ketron® 1000 PEEK unfilled, extruded (ISO Data)
Ketron PEEK-1000 stock shapes are produced from virgin polyetheretherketone resin and offer the highest toughness and impact strength of all Ketron PEEK grades. Both Ketron PEEK-1000 natural & black..
Limiting Pressure Velocity 0.330 MPa-m/sec
9420 psi-ft/min
without lubrication; MPC Test
Manifattura Cattaneo PA 6.6 30% GF Nylon, Glass Filled
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.