Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.280 MPa-m/sec | 8000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Fluorosint® 207 PTFE, Compression Molded Synthetic Mica-filled PTFE (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.280 MPa-m/sec | 8000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Fluorosint® 500 PTFE, synthetic mica-filled PTFE, compression molded (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.280 MPa-m/sec | 7990 psi-ft/min | at 0.35 m/s |
A. Schulman ComAlloy Lubrilon® 62S1 Internally Lubricated, Nylon 6/6 Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |