Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 989.74 MPa @Strain 0.200 % |
143550 psi @Strain 0.200 % |
hardened |
Wieland Simidur S 2 PFM Alloy Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental |