Polymer Property : Tensile Strength, Yield = 9500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.5 MPa

@Thickness 1.57 mm
9500 psi

@Thickness 0.0620 in
CW; ASTM D638
Industrial Laminates/Norplex NP325 Cotton Fabric
Description: Linen phenolic laminate with graphite added as a solid lubricant. Linen substrate provides better machining and wear resistance than NP315.Thickness Tested: 0.062", 0.125" and 0.500".
Tensile Strength, Yield 65.5 MPa

@Thickness 1.57 mm
9500 psi

@Thickness 0.0620 in
CW; ASTM D638
Industrial Laminates/Norplex NP344 Cotton Fabric
Description: Fine weave canvas laminate with high temperature phenolic resin and molybdenum disulfide lubricant. Good machining properties and low coefficient of thermal expansion. Better machining ..