Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 65.5 MPa @Thickness 1.57 mm |
9500 psi @Thickness 0.0620 in |
CW; ASTM D638 |
Industrial Laminates/Norplex NP325 Cotton Fabric Description: Linen phenolic laminate with graphite added as a solid lubricant. Linen substrate provides better machining and wear resistance than NP315.Thickness Tested: 0.062", 0.125" and 0.500". |
|||
Tensile Strength, Yield | 65.5 MPa @Thickness 1.57 mm |
9500 psi @Thickness 0.0620 in |
CW; ASTM D638 |
Industrial Laminates/Norplex NP344 Cotton Fabric Description: Fine weave canvas laminate with high temperature phenolic resin and molybdenum disulfide lubricant. Good machining properties and low coefficient of thermal expansion. Better machining .. |