Mechanical Properties Metric English Comments
Tensile Strength, Yield 917 MPa

@Strain 0.200 %
133000 psi

@Strain 0.200 %
Transverse
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Age Hardened Round
Tensile strength (ultimate and yield), hardness, impact, and elongation values reported here are typical for Age Hardened Round samples. Other property values are typical of INCONEL® alloy 725.D..