Mechanical Properties Metric English Comments
Tensile Strength, Yield 917 MPa

@Strain 0.200 %
133000 psi

@Strain 0.200 %
Transverse
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Age Hardened Round
Tensile strength (ultimate and yield), hardness, impact, and elongation values reported here are typical for Age Hardened Round samples. Other property values are typical of INCONEL® alloy 725.D..
Tensile Strength, Yield 915 MPa

@Temperature 23.0 °C
133000 psi

@Temperature 73.4 °F
ATI Allegheny Ludlum Stainless Steel Type 201L, 20% Cold Work (UNS S20103)
Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese ..