Mechanical Properties Metric English Comments
Tensile Strength, Yield 82.0 MPa

@Strain 0.200 %,
Temperature 600 °C
11900 psi

@Strain 0.200 %,
Temperature 1110 °F
EN min.; EN 10002-5
Outokumpu 4828 High Temperature Austenitic Stainless Steel
Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and ..
Tensile Strength, Yield 82.0 MPa

@Strain 0.200 %,
Temperature 600 °C
11900 psi

@Strain 0.200 %,
Temperature 1110 °F
EN min.; EN 10002-5
Outokumpu 4833 High Temperature Austenitic Stainless Steel
Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and ..
Tensile Strength, Yield 82.0 MPa

@Strain 0.200 %,
Temperature 600 °C
11900 psi

@Strain 0.200 %,
Temperature 1110 °F
EN min.; EN 10002-5
Outokumpu 4845 High Temperature Austenitic Stainless Steel
Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o..
Tensile Strength, Yield 82.0 MPa

@Temperature 23.0 °C
11900 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66  (Unverified Data**)
Zytel® 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
Tensile Strength, Yield 82.0 MPa

@Temperature 23.0 °C
11900 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 101L BKB080 Nylon 66  (Unverified Data**)
Zytel® 101L BKB080 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength, Yield 82.0 MPa

@Temperature 649 °C
11900 psi

@Temperature 1200 °F
ATI Allegheny Ludlum AL 453™ Stainless Steel
Single phase iron-chromium ferritic stainless steel alloy. Should be annealed between 1450 and 1600°F and quickly cooled. Information provided by Allegheny Ludlum
Tensile Strength, Yield 82.0 MPa

@Temperature 371 °C
11900 psi

@Temperature 700 °F
ATI Wah Chang Zircadyne® Alloy Zr 702
Zircadyne 702 is commercially pure zirconium. Alloy exhibits good ductility even at cryogenic temperatures and good strength comparable with other common engineering alloys.Information provided by A..
Tensile Strength, Yield 82.0 MPa

@Temperature 23.0 °C
11900 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® FG101L NC010 Nylon 66  (Unverified Data**)
Zytel® FG101L NC010 is a lubricated polyamide 66 resin for injection molding. It has been developed for consideration into applications such as parts for the food industry.Information provided by D..