Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 80.0 MPa @Temperature 23.0 °C |
11600 psi @Temperature 73.4 °F |
DAM; ASTM D638 |
DuPont Performance Polymers Zytel® 7304 NC010 Nylon 6
(Unverified Data**) Zytel® 7304 NC010 is a medium viscosity, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | >= 80.0 MPa @Strain 0.200 %, Thickness 4.00 - 12.5 mm |
>= 11600 psi @Strain 0.200 %, Thickness 0.157 - 0.492 in |
Temper H111; Standard EN 485-2 |
Constellium PLAN 5754 Aluminum Rolled Plate Rolled plates in 5754 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 5754 PLAN is mainly used for low stressed mechanical components, manufactured by intensive m.. |
|||
Tensile Strength, Yield | >= 80.0 MPa @Strain 0.200 %, Thickness 4.00 - 12.5 mm |
>= 11600 psi @Strain 0.200 %, Thickness 0.157 - 0.492 in |
Temper H111; Standard EN 485-2 |
Constellium PLAN OX 5754 Aluminum Rolled Plate Rolled plates in 5754 PLAN OX are optimized for minimum residual stress, improved dimensional tolerances and for decorative* anodizing. 5754 PLAN OX is mainly used for low stressed, anodized compone.. |
|||
Tensile Strength, Yield | 80.0 MPa @Temperature 23.0 °C |
11600 psi @Temperature 73.4 °F |
DAM; ASTM D638 |
DuPont Performance Polymers Zytel® 7301 NC010 Nylon 6
(Unverified Data**) Zytel® 7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 80.0 MPa @Temperature 23.0 °C |
11600 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 7301 NC010 Nylon 6
(Unverified Data**) Zytel® 7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 80.0 MPa @Temperature 23.0 °C |
11600 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® FG7301 NC010 Nylon 6
(Unverified Data**) Zytel® FG7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications. It has been developed for consideration into applications such as parts for the food industry.In.. |