Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 8.432 MPa @Temperature -54.0 °C |
1223 psi @Temperature -65.2 °F |
Flatwise TS |
Hexcel® HexPly® F185 Epoxy Resin, 1581 Glass Fabric Hexcel designation: 1581-38"-F185; Fiber: 150-1/2Information provided by HexCel |