Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 79.0 MPa @Temperature 23.0 °C |
11500 psi @Temperature 73.4 °F |
ASTM D638 |
BASF Ultramid® 8202 L Intermediate PA6 (Dry) Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is avai.. |