Mechanical Properties Metric English Comments
Tensile Strength, Yield 544 MPa

@Strain 0.200 %
78900 psi

@Strain 0.200 %
10% Cold Worked
AK Steel 439 ULTRA FORM® Stainless Steel
AK Steel 439 ULTRA FORM™ was developed for applications requiring oxidation and corrosion resistance superior to Type 409 as well as superior formability to AK Steel 439 Stainless Steel. As a resul..
Tensile Strength, Yield 544 MPa

@Strain 0.200 %,
Temperature 400 °C
78900 psi

@Strain 0.200 %,
Temperature 752 °F
Special Metals NIMONIC® alloy 91 Ni-Cr-Co Alloy
NIMONIC® alloy 91 is a wrought nickel-chromium-cobalt based alloy strengthened by additions of aluminum and titanium.This alloy is a modification of NIMONIC alloy 90, but has an increased chromium ..