Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 544 MPa @Strain 0.200 % |
78900 psi @Strain 0.200 % |
10% Cold Worked |
AK Steel 439 ULTRA FORM® Stainless Steel AK Steel 439 ULTRA FORM™ was developed for applications requiring oxidation and corrosion resistance superior to Type 409 as well as superior formability to AK Steel 439 Stainless Steel. As a resul.. |
|||
Tensile Strength, Yield | 544 MPa @Strain 0.200 %, Temperature 400 °C |
78900 psi @Strain 0.200 %, Temperature 752 °F |
|