Polymer Property : Tensile Strength, Yield = 72500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 500 MPa

@Strain 0.200 %
72500 psi

@Strain 0.200 %
Outokumpu Typical, Annealed Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4021 Martensitic Stainless Steel
Moderate corrosion resistant stainless steel hardenable up to 1000N/mm2. Re-sulphurized steel improves machining properties.Applications: ShaftsKnivesFastenersSurgical applicationsDomestic applicat..
Tensile Strength, Yield 500 MPa

@Strain 0.200 %,
Temperature 850 °C
72500 psi

@Strain 0.200 %,
Temperature 1560 °F
Special Metals UDIMET® alloy 520 Superalloy
UDIMET® alloy 520 is a precipitation-hardenable nickel base superalloy with an exceptional combination of high-temperature mechanical properties, corrosion resistance and forgeability characteris..
Tensile Strength, Yield >= 500 MPa

@Strain 0.200 %,
Temperature 300 °C
>= 72500 psi

@Strain 0.200 %,
Temperature 572 °F
ThyssenKrupp N-A-XTRA® 620 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Tensile Strength, Yield 500 MPa

@Strain 0.200 %
72500 psi

@Strain 0.200 %
after porcelain firing
Wieland BioPorta G PFM Alloy
Gold-platinum ceramic alloyApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneering, acrylic veneeringDental
Tensile Strength, Yield 500 MPa

@Thickness 203 - 305 mm
72500 psi

@Thickness 8.00 - 12.0 in
at center (L/T direction)
Alcoa QC-10® Aluminum Mold Alloy
Specifically designed for high production injection and blow mold applications, QC-10 offers outstanding strength, stability, and durability. Its improved alloy composition provides outstanding, 1"-..
Tensile Strength, Yield 500 MPa

@Strain 0.200 %,
Thickness 25.0 - 60.0 mm
72500 psi

@Strain 0.200 %,
Thickness 0.984 - 2.36 in
Typical Strength
Constellium ALPLAN® 7075 High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 7075 precision plates combine a good dimensional stability with high mechanical strength. Both the outstanding flatness and the low roughness of the surfaces, protected by a plastic film, m..
Tensile Strength, Yield 500 MPa

@Strain 0.200 %,
Thickness 40.0 - 50.0 mm
72500 psi

@Strain 0.200 %,
Thickness 1.57 - 1.97 in
Typical Strength
Constellium Fortal® Aluminum Alloy
Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m..
Tensile Strength, Yield 500 MPa

@Strain 0.200 %
72500 psi

@Strain 0.200 %
As-HIP
Crucible Compaction Metals P/M 625M Corrosion Resistant Alloy
P/M 625M (chemically, UNS N07626) is produced by the state-of-the-art Crucible P/M process: inert gas atomization, coupled with consolidation by hot isostatic pressing (HIP) and/or extrusion. The a..
Tensile Strength, Yield 500 MPa

@Strain 0.200 %,
Time 1.80e+6 sec
72500 psi

@Strain 0.200 %,
Time 500 hour
Room Temperature properties after Isothermal Exposure
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy
INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar..
Tensile Strength, Yield 500 MPa

@Strain 0.200 %,
Treatment Temp. 650 °C
72500 psi

@Strain 0.200 %,
Treatment Temp. 1200 °F
Room Temperature properties after Isothermal Exposure
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy
INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar..