Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 500 MPa @Strain 0.200 % |
72500 psi @Strain 0.200 % |
Outokumpu Typical, Annealed Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4021 Martensitic Stainless Steel Moderate corrosion resistant stainless steel hardenable up to 1000N/mm2. Re-sulphurized steel improves machining properties.Applications: ShaftsKnivesFastenersSurgical applicationsDomestic applicat.. |
|||
Tensile Strength, Yield | 500 MPa @Strain 0.200 %, Temperature 850 °C |
72500 psi @Strain 0.200 %, Temperature 1560 °F |
|
Special Metals UDIMET® alloy 520 Superalloy UDIMET® alloy 520 is a precipitation-hardenable nickel base superalloy with an exceptional combination of high-temperature mechanical properties, corrosion resistance and forgeability characteris.. |
|||
Tensile Strength, Yield | >= 500 MPa @Strain 0.200 %, Temperature 300 °C |
>= 72500 psi @Strain 0.200 %, Temperature 572 °F |
|
ThyssenKrupp N-A-XTRA® 620 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Tensile Strength, Yield | 500 MPa @Strain 0.200 % |
72500 psi @Strain 0.200 % |
after porcelain firing |
Wieland BioPorta G PFM Alloy Gold-platinum ceramic alloyApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneering, acrylic veneeringDental |
|||
Tensile Strength, Yield | 500 MPa @Thickness 203 - 305 mm |
72500 psi @Thickness 8.00 - 12.0 in |
at center (L/T direction) |
Alcoa QC-10® Aluminum Mold Alloy Specifically designed for high production injection and blow mold applications, QC-10 offers outstanding strength, stability, and durability. Its improved alloy composition provides outstanding, 1"-.. |
|||
Tensile Strength, Yield | 500 MPa @Strain 0.200 %, Thickness 25.0 - 60.0 mm |
72500 psi @Strain 0.200 %, Thickness 0.984 - 2.36 in |
Typical Strength |
Constellium ALPLAN® 7075 High-Strength Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 7075 precision plates combine a good dimensional stability with high mechanical strength. Both the outstanding flatness and the low roughness of the surfaces, protected by a plastic film, m.. |
|||
Tensile Strength, Yield | 500 MPa @Strain 0.200 %, Thickness 40.0 - 50.0 mm |
72500 psi @Strain 0.200 %, Thickness 1.57 - 1.97 in |
Typical Strength |
Constellium Fortal® Aluminum Alloy Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m.. |
|||
Tensile Strength, Yield | 500 MPa @Strain 0.200 % |
72500 psi @Strain 0.200 % |
As-HIP |
Crucible Compaction Metals P/M 625M Corrosion Resistant Alloy P/M 625M (chemically, UNS N07626) is produced by the state-of-the-art Crucible P/M process: inert gas atomization, coupled with consolidation by hot isostatic pressing (HIP) and/or extrusion. The a.. |
|||
Tensile Strength, Yield | 500 MPa @Strain 0.200 %, Time 1.80e+6 sec |
72500 psi @Strain 0.200 %, Time 500 hour |
Room Temperature properties after Isothermal Exposure |
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar.. |
|||
Tensile Strength, Yield | 500 MPa @Strain 0.200 %, Treatment Temp. 650 °C |
72500 psi @Strain 0.200 %, Treatment Temp. 1200 °F |
Room Temperature properties after Isothermal Exposure |
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar.. |