Polymer Property : Tensile Strength, Yield = 71500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 493 MPa

@Strain 0.200 %,
Thickness 12.7 mm
71500 psi

@Strain 0.200 %,
Thickness 0.500 in
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 1000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Tensile Strength, Yield 493 MPa

@Diameter 12.7 mm,
Temperature 25.0 °C
71500 psi

@Diameter 0.500 in,
Temperature 77.0 °F
0.2% offset
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..