Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 493 MPa @Strain 0.200 %, Thickness 12.7 mm |
71500 psi @Strain 0.200 %, Thickness 0.500 in |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Tensile Strength, Yield | 493 MPa @Diameter 12.7 mm, Temperature 25.0 °C |
71500 psi @Diameter 0.500 in, Temperature 77.0 °F |
0.2% offset |
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |