Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 7.90 MPa

@Strain 5.00 %
1150 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® PL460-S 46 Shore D Copolyester Elastomer, Injection Grade (Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 7.90 MPa

@Strain 5.00 %
1150 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® PL460-S 46 Shore D, Injection Grade, Flame Retardant Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..