Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 472 MPa

@Strain 0.200 %,
Thickness 1.45 mm
68500 psi

@Strain 0.200 %,
Thickness 0.0571 in
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 16000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Tensile Strength, Yield >= 472 MPa

@Strain 0.200 %,
Thickness 127 - 152.4 mm
>= 68500 psi

@Strain 0.200 %,
Thickness 5.00 - 6.000 in
Tempers T651 / T652
Constellium Alumold® 500 Rolled Aluminum
The Alumold® 500 alloy has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important prop..