Tensile Strength, Yield >= 435 MPa

@Strain 0.200 %,
Thickness 254 - 305 mm
>= 63100 psi

@Strain 0.200 %,
Thickness 10.0 - 12.0 in
Tempers T651 / T652
Constellium Alumold® 500 Rolled Aluminum