Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 433 MPa @Temperature 232 °C |
62800 psi @Temperature 450 °F |
|
Hexcel® HexPly® F650 Bismaleimide Resin with Quartz 581 fabric reinforcement Laminate Physicals: 55.4% Fiber volume, 31.4% Resin content, 0.7% Voids, 1.78% gm.cc Specific gravityInformation provided by HexCel |