Polymer Property : Tensile Strength, Yield = 433 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 433 MPa

@Temperature 232 °C
62800 psi

@Temperature 450 °F
Hexcel® HexPly® F650 Bismaleimide Resin with Quartz 581 fabric reinforcement
Laminate Physicals: 55.4% Fiber volume, 31.4% Resin content, 0.7% Voids, 1.78% gm.cc Specific gravityInformation provided by HexCel