Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.10 MPa

@Strain 50.0 %
595 psi

@Strain 50.0 %
ASTM D412
GRECO ISOTHANE 3080A Polyether TPU Resin
ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod..
Tensile Strength, Yield 4.10 MPa

@Strain 50.0 %
595 psi

@Strain 50.0 %
ASTM D412
GRECO ISOTHANE 1085A Poly(adipate)ester TPU Resin
ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products ..
Tensile Strength, Yield 4.10 MPa

@Strain 50.0 %
595 psi

@Strain 50.0 %
ASTM D412
GRECO ISOTHANE 1085AF Poly(adipate)ester TPU Resin
ISOTHANE 1000 FDA series products are poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance and solvent resistance. These products can be inject..