Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.10 MPa @Strain 50.0 % |
595 psi @Strain 50.0 % |
ASTM D412 |
GRECO ISOTHANE 3080A Polyether TPU Resin ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod.. |
|||
Tensile Strength, Yield | 4.10 MPa @Strain 50.0 % |
595 psi @Strain 50.0 % |
ASTM D412 |
GRECO ISOTHANE 1085A Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products .. |
|||
Tensile Strength, Yield | 4.10 MPa @Strain 50.0 % |
595 psi @Strain 50.0 % |
ASTM D412 |
GRECO ISOTHANE 1085AF Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 FDA series products are poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance and solvent resistance. These products can be inject.. |