Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 57.9 MPa @Thickness 1.57 mm |
8400 psi @Thickness 0.0620 in |
CW; ASTM D638 |
Industrial Laminates/Norplex NP615 Paper Base Laminate Description: Room temperature punching and shearing grade up to .125" thick. More flexible and lower mechanical properties than NP611. NP615 is produced with high resin content melamine impregnated .. |
|||
Tensile Strength, Yield | 57.9 MPa @Thickness 1.57 mm |
8400 psi @Thickness 0.0620 in |
CW; ASTM D638 |
Industrial Laminates/Norplex NP612 Paper Base Laminate Description: Room temperature punching and shearing grade up to .125" thick. More flexible and lower mechanical properties than NP611. Intended for applications where electrical and moisture require.. |
|||
Tensile Strength, Yield | 57.9 MPa @Temperature 25.0 °C |
8400 psi @Temperature 77.0 °F |
Quasi tensile strength |
Hexcel® HexPly® 8551-7 Epoxy Matrix, IM7 Fiber Information provided by HexCel |
|||
Tensile Strength, Yield | 57.9 MPa @Strain 0.200 %, Temperature 871 °C |
8400 psi @Strain 0.200 %, Temperature 1600 °F |
Longitudinal |
AK Steel NITRONIC® 19-D Duplex Stainless Steel AK Steel NITRONIC® 19D is a stainless steel with a mixed ferrite and austenite structure. This alloy provides high yield strength (65 ksi minimum {448 MPa}),
good drawing and welding characteristi.. |