Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 3.92 MPa @Strain 5.00 % |
569 psi @Strain 5.00 % |
ASTM D638 |
SK Chemicals SKYPEL P147D Productivity Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Tensile Strength, Yield | 3.92 MPa @Strain 300 % |
569 psi @Strain 300 % |
ASTM D412 |
SK Chemicals SKYTHANE® 850A T series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Yield | 3.92 MPa @Strain 5.00 % |
569 psi @Strain 5.00 % |
ASTM D638 |
Samyang Triel® 5401BM Thermoplastics Polyetherester Elastomer, Blow Molding Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5401BM is for blow molding applications.Applications: Automotive - CVJB and BellowsInformation provided .. |
|||
Tensile Strength, Yield | 3.92 MPa @Strain 5.00 % |
569 psi @Strain 5.00 % |
ASTM D638 |
Samyang Triel® 5501BM Thermoplastics Polyetherester Elastomer, Blow Molding Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5501BM is for blow molding applications.Applications: Automotive BellowsInformation provided by Samyang... |
|||
Tensile Strength, Yield | 3.92 MPa @Strain 10.0 % |
569 psi @Strain 10.0 % |
ASTM D638 |
SK Chemicals SKYPEL P137DW Productivity Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Tensile Strength, Yield | 3.92 MPa @Strain 300 % |
569 psi @Strain 300 % |
ASTM D412 |
SK Chemicals SKYTHANE® 410 Hotmelt Grade UB Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Yield | 3.92 MPa @Strain 100 % |
569 psi @Strain 100 % |
ASTM D412 |
SK Chemicals SKYTHANE® 420 Hotmelt Grade UB Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Yield | 3.92 MPa @Strain 100 % |
569 psi @Strain 100 % |
ASTM D412 |
SK Chemicals SKYTHANE® 470A T series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Yield | 3.92 MPa @Strain 100 % |
569 psi @Strain 100 % |
ASTM D412 |
SK Chemicals SKYTHANE® 385A S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |