Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 296 - 386 MPa @Strain 0.200 %, Thickness 1.02 - 2.92 mm |
42900 - 56000 psi @Strain 0.200 %, Thickness 0.0400 - 0.115 in |
|
ATI Allegheny Ludlum 430 Ferritic Stainless Steel Characteristics:oxidation resistant at elevated temperatures, corrosion resistance approaching nickel-bearing stainless steels in mildly corrosive environments, ductile, does not work harden readily.. |