Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 490 MPa @Temperature 149 °C |
71000 psi @Temperature 300 °F |
0° Direction, Wet; ASTM D638 |
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 4503 Quartz Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |
|||
Tensile Strength, Yield | 490 MPa @Thickness 1.57 mm |
71000 psi @Thickness 0.0620 in |
CW; ASTM D638 |
Industrial Laminates/Norplex NP545 Carbon Fiber
(discontinued **) Description: NP545 is composed of carbon fiber fabric and an epoxy resin system. It has excellent moisture resistance and physical properties. Potential uses include fixtures and gage systems, high .. |
|||
Tensile Strength, Yield | 490 MPa @Temperature 871 °C, Time 45700 sec |
71100 psi @Temperature 1600 °F, Time 12.7 hour |
As Welded, Solution Annealed, and Aged; Weld/Weld Fracture; 0.2% Offset |
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Tensile Strength, Yield | 490 MPa @Strain 0.200 %, Thickness 203.2 - 254 mm |
71100 psi @Strain 0.200 %, Thickness 8.000 - 10.0 in |
Typical Strength |
Constellium Alumold® 500 Rolled Aluminum The Alumold® 500 alloy has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important prop.. |
|||
Tensile Strength, Yield | 490 MPa @Strain 0.200 %, Thickness 100 - 140 mm |
71100 psi @Strain 0.200 %, Thickness 3.94 - 5.51 in |
Typical Strength |
Constellium Certal® Thick Aluminum Plate Certal® thick plates have been optimized to provide excellent machinability, shape stability and high strength. Certal® is therefore ideal for industrial tools. Applications include injection and .. |
|||
Tensile Strength, Yield | >= 490 MPa @Strain 1.00 % |
>= 71100 psi @Strain 1.00 % |
|
Industeel URANUS® 45N 22Cr 3Mo Duplex Stainless Steel with PREN = 33 or 34 Description: URANUS® 45N (UR 45N) is a nitrogen alloyed (= 0.15%) austenitic-ferritic stainless steel (22.05 type) with improved structure stability and high general, localized and stress corrosion.. |