Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 470 MPa

@Temperature 20.0 °C
>= 68200 psi

@Temperature 68.0 °F
Condition T6 (Quenching in water at RT)
PEAK Werkstoff DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition T6
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Tensile Strength, Yield >= 470 MPa

@Strain 0.200 %,
Temperature 400 °C
>= 68200 psi

@Strain 0.200 %,
Temperature 752 °F
ThyssenKrupp N-A-XTRA® 620 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Tensile Strength, Yield 470 MPa

@Thickness 356 - 457 mm
68200 psi

@Thickness 14.0 - 18.0 in
at center (L/T direction)
Alcoa QC-10® Aluminum Mold Alloy
Specifically designed for high production injection and blow mold applications, QC-10 offers outstanding strength, stability, and durability. Its improved alloy composition provides outstanding, 1"-..
Tensile Strength, Yield >= 470 MPa

@Strain 0.200 %,
Thickness 12.5 - 25.0 mm
>= 68200 psi

@Strain 0.200 %,
Thickness 0.492 - 0.984 in
Temper T651; Standard EN 485-2
Constellium ALPLAN® 7075 High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 7075 precision plates combine a good dimensional stability with high mechanical strength. Both the outstanding flatness and the low roughness of the surfaces, protected by a plastic film, m..
Tensile Strength, Yield 470 MPa

@Strain 0.200 %,
Thickness 254 - 305 mm
68200 psi

@Strain 0.200 %,
Thickness 10.0 - 12.0 in
Typical Strength
Constellium Alumold® 500 Rolled Aluminum
The Alumold® 500 alloy has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important prop..
Tensile Strength, Yield >= 470 MPa

@Strain 0.200 %,
Thickness 40.0 - 50.0 mm
>= 68200 psi

@Strain 0.200 %,
Thickness 1.57 - 1.97 in
Constellium Fortal® Aluminum Alloy
Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m..