Mechanical Properties Metric English Comments
Tensile Strength, Yield 320 MPa

@Strain 1.00 %
46400 psi

@Strain 1.00 %
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4306 Cr-Ni Austenitic Stainless Steel
General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll..
Tensile Strength, Yield 320 MPa

@Strain 1.00 %
46400 psi

@Strain 1.00 %
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4307 Cr-Ni Austenitic Stainless Steel
General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll..
Tensile Strength, Yield 320 MPa

@Strain 0.200 %
46400 psi

@Strain 0.200 %
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Tensile Strength, Yield 320 MPa

@Strain 1.00 %
46400 psi

@Strain 1.00 %
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4401 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Yield 320 MPa

@Strain 1.00 %
46400 psi

@Strain 1.00 %
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Yield 320 MPa

@Strain 0.200 %
46400 psi

@Strain 0.200 %
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4406 Cr-Ni-Mo Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Tensile Strength, Yield 320 MPa

@Strain 1.00 %
46400 psi

@Strain 1.00 %
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4432 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Yield 320 MPa

@Strain 0.200 %
46400 psi

@Strain 0.200 %
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4713 High Temperature Ferritic Stainless Steel
Does not form brittle phases but should only be exposed to moderately corrosive atmospheres due to low chromium content.Applications: Mostly used in high temperature applications with sulphurous atm..
Tensile Strength, Yield >= 320 MPa

@Strain 1.00 %
>= 46400 psi

@Strain 1.00 %
Industeel CLC 17.13.3 LN Nitrogen Containing 18Cr-10Ni-2Mo Austenitic Stainless Steel
Description: CLC 17-13-3LN is a nitrogen alloyed austenitic stainless steel with Mo additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior water ..
Tensile Strength, Yield >= 320 MPa

@Strain 0.200 %
>= 46400 psi

@Strain 0.200 %
Industeel URANUS® B26 6 Mo High Performance Super-Austenitic Stainless Steel with PREN = 43
Description: URANUS® B26 (UR B26) is a 25% Ni, 20% Cr, 6% Mo superaustenitic stainless steel grade with 0.2 % nitrogen additions, particularly designed for high structural stability and high corr..
Tensile Strength, Yield >= 320 MPa

@Strain 0.200 %,
Thickness <=7.938 mm
>= 46400 psi

@Strain 0.200 %,
Thickness <=0.3125 in
per ASTM A240; transverse
American Utility Metals Cromgard® Stainless Steel
Cromgard is a low cost stainless steel, which is able to provide benefits of good weldability and formability, making it capable of fabrication by conventional techniques. It provides the benefits o..
Tensile Strength, Yield 320 MPa

@Strain 0.200 %
46400 psi

@Strain 0.200 %
Typical
Aleris Weldural Aluminum Alloy, 300 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..
Tensile Strength, Yield 320 MPa

@Thickness 1.70 mm,
Temperature 427 °C
46400 psi

@Thickness 0.0669 in,
Temperature 801 °F
0.2% offset
Haynes Hastelloy® C-4 alloy, sheet, heat treated at 1066°C, rapid quenched
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..
Tensile Strength, Yield 320 MPa

@Thickness 3.20 mm,
Temperature 204 °C
46400 psi

@Thickness 0.126 in,
Temperature 399 °F
0.2% offset
Haynes Hastelloy® C-4 alloy, sheet, heat treated at 1066°C, rapid quenched
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..
Tensile Strength, Yield 320 MPa

@Strain 1.00 %
46400 psi

@Strain 1.00 %
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 725LN Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form.
Tensile Strength, Yield 320 MPa

@Strain 0.200 %,
Temperature 250 °C
46400 psi

@Strain 0.200 %,
Temperature 482 °F
EN min.; EN 10002-5
Outokumpu LDX 2101® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..