Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 315 MPa @Strain 0.200 %, Temperature 200 °C |
45700 psi @Strain 0.200 %, Temperature 392 °F |
EN min.; EN 10002-5 |
Outokumpu 2205 Duplex Stainless Steel Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t.. |
|||
Tensile Strength, Yield | 315 MPa @Strain 1.00 %, Temperature 50.0 °C |
45700 psi @Strain 1.00 %, Temperature 122 °F |
EN min.; EN 10002-5 |
Outokumpu 253MA® High Temperature Austenitic Stainless Steel Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be.. |
|||
Tensile Strength, Yield | 315 MPa @Strain 1.00 % |
45700 psi @Strain 1.00 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4841 High Temperature Austenitic Stainless Steel Variant of 1.4845 with an increased silicon content which enhances the steel's resistance to oxidation/corrosion but has also made it more susceptible to embrittlement.Applications: Heat and creep r.. |
|||
Tensile Strength, Yield | >= 315 MPa @Strain 1.00 % |
>= 45700 psi @Strain 1.00 % |
|
Industeel CLC 17.13.5 LN Modified 317LN Mo 4% Austenitic Stainless Steel Description: CLC 17-13-5LN (317LNM) is a Nitrogen alloyed austenitic stainless steel with a high Molybdenum addition (=4%). Alloy CLC 17-13-5LN (317LNM) exhibits austenitic microstructure free of de.. |
|||
Tensile Strength, Yield | >= 315 MPa @Strain 1.00 % |
>= 45700 psi @Strain 1.00 % |
|
Industeel CLC 18.12.4 LN 3%Mo Austenitic Stainless Steel with Nitrogen Addition Description: CLC 18-12-4LN (317LN) is a Nitrogen alloyed austenitic stainless steel with a 3% Mo minimum addition (>4%). Alloys CLC 18-12-4LN (317LN) exhibit austenitic microstructure free of delete.. |
|||
Tensile Strength, Yield | 315 MPa @Strain 0.200 %, Thickness 203.2 - 254 mm |
45700 psi @Strain 0.200 %, Thickness 8.000 - 10.0 in |
Typical Strength |
Constellium Alumold® 350 Aluminum Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti.. |
|||
Tensile Strength, Yield | 315 MPa @Thickness 1.60 mm |
45700 psi @Thickness 0.0630 in |
L Direction |
Aleris AA5024-H116 Aluminum Magnesium Scandium Alloy Features good weldability, excellent damage tolerance, good corrosion resistance, creep-formability. Aleris AlMgSc alloy AA5024 H116 allows simplification of the manufacturing process of aircraft f.. |
|||
Tensile Strength, Yield | 315 MPa @Strain 0.200 %, Temperature 900 °C |
45700 psi @Strain 0.200 %, Temperature 1650 °F |
|
Special Metals NIMONIC® alloy 91 Ni-Cr-Co Alloy NIMONIC® alloy 91 is a wrought nickel-chromium-cobalt based alloy strengthened by additions of aluminum and titanium.This alloy is a modification of NIMONIC alloy 90, but has an increased chromium .. |