Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.0 MPa

@Strain 300 %
4200 psi

@Strain 300 %
ASTM D412
Teknor Apex Laripur® LPR 5260EG Thermoplastic Polyurethane
Features: - Excellent performance under extreme and aggressive environments - Superior abrasion and cut resistance - Resistance to chemical, microbial attack and hydrolysis - Excellent flexibility a..