Mechanical Properties Metric English Comments
Tensile Strength, Yield 372 MPa

@Temperature 23.9 °C
54000 psi

@Temperature 75.0 °F
0° Direction, Dry; Oven Cure, 90min, 260°F; ASTM D638
Park Electrochemical Nelcote® F-529 Phenolic Prepreg, 7781 E-Glass Reinforced
Nelcote® F-529 is a non-halogenated phenolic resin designed specifically for use in aircraft and mass-transit interior laminate and sandwich panels. F-529 was formulated for applications requiring ..
Tensile Strength, Yield 372 MPa

@Strain 0.200 %,
Thickness 12.7 mm
54000 psi

@Strain 0.200 %,
Thickness 0.500 in
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 16000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Tensile Strength, Yield 372 MPa

@Thickness 25.4 mm,
Temperature 20.0 °C
54000 psi

@Thickness 1.00 in,
Temperature 68.0 °F
0.2% offset
Haynes Hastelloy® C-2000® alloy, flat products
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Tensile Strength, Yield 372 MPa

@Thickness 23.4 mm,
Temperature 20.0 °C
54000 psi

@Thickness 0.921 in,
Temperature 68.0 °F
0.2% offset
Haynes Hastelloy® C-22® alloy, transverse, GMAW short arc weldment, plate
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..