Tensile Strength, Yield 248 MPa

@Temperature 121 °C
36000 psi

@Temperature 250 °F
0° Direction, Dry; ASTM D638 Type 1
Park Electrochemical Nelcote® P-650M Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-650M is a polyester resin system suitable for coating on any MIL-C-9084. P-650M has good electrical and mechanical properties and has been used in a wide variety of applications, includi..
Tensile Strength, Yield 248 MPa

@Thickness 6.35 mm,
Temperature 538 °C
36000 psi

@Thickness 0.250 in,
Temperature 1000 °F
0.2% offset
Haynes Hastelloy® C-22® alloy, transverse, GTAW weldment, sheet - plate
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Tensile Strength, Yield 248 MPa

@Strain 0.200 %,
Temperature 204 °C
36000 psi

@Strain 0.200 %,
Temperature 399 °F
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Tensile Strength, Yield 248 MPa

@Strain 0.200 %
36000 psi

@Strain 0.200 %
ATI Allegheny Ludlum 316Ti Austenitic Stainless Steel
Characteristics:excellent resistance to general corrosion, excellent resistance to pitting/crevice corrosion, resistant to sensitization, better creep stress-rupture and tensile strength at elevated..
Tensile Strength, Yield 248 MPa

@Strain 0.200 %,
Temperature 204 °C
36000 psi

@Strain 0.200 %,
Temperature 399 °F
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is..