Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 248 MPa @Temperature 121 °C |
36000 psi @Temperature 250 °F |
0° Direction, Dry; ASTM D638 Type 1 |
Park Electrochemical Nelcote® P-650M Polyester Prepreg, 7781 E-Glass Reinforced Nelcote® P-650M is a polyester resin system suitable for coating on any MIL-C-9084. P-650M has good electrical and mechanical properties and has been used in a wide variety of applications, includi.. |
|||
Tensile Strength, Yield | 248 MPa @Thickness 6.35 mm, Temperature 538 °C |
36000 psi @Thickness 0.250 in, Temperature 1000 °F |
0.2% offset |
Haynes Hastelloy® C-22® alloy, transverse, GTAW weldment, sheet - plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Yield | 248 MPa @Strain 0.200 %, Temperature 204 °C |
36000 psi @Strain 0.200 %, Temperature 399 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Tensile Strength, Yield | 248 MPa @Strain 0.200 % |
36000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum 316Ti Austenitic Stainless Steel Characteristics:excellent resistance to general corrosion, excellent resistance to pitting/crevice corrosion, resistant to sensitization, better creep stress-rupture and tensile strength at elevated.. |
|||
Tensile Strength, Yield | 248 MPa @Strain 0.200 %, Temperature 204 °C |
36000 psi @Strain 0.200 %, Temperature 399 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |