Polymer Property : Tensile Strength, Yield = 3190 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.0 MPa

@Strain 0.200 %,
Temperature 816 °C
3190 psi

@Strain 0.200 %,
Temperature 1500 °F
AK Steel 409 ULTRA FORM® Stainless Steel
AK Steel 409 ULTRA FORM Stainless Steel provides an outstanding combination of improved forming and welding characteristics, while providing superior resistance to oxidation, corrosion, ridging and ..
Tensile Strength, Yield 22.0 MPa

@Strain 100 %
3190 psi

@Strain 100 %
ASTM D-412
BASF Elastollan® S60D Polyester Type Polyurethane Elastomer
Recommended for injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fuel and solv..
Tensile Strength, Yield 22.0 MPa

@Strain 100 %
3190 psi

@Strain 100 %
ASTM D-412
BASF Elastollan® 1160D Polyether Type Polyurethane Elastomer
Recommended for injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exh..
Tensile Strength, Yield 22.0 MPa

@Strain 300 %
3190 psi

@Strain 300 %
ASTM D-412
BASF Elastollan® C-90A Polyester Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen..