Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Elastollan® S60D Polyester Type Polyurethane Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer BASF
Trade Name Elastollan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Elastollan® S60D Polyester Type Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Recommended for injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fuel and solvent resistance. These products can be injection and blow molded and extruded. As with all TPU products this grade must be dried prior to processing.Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength, Ultimate 43.0 MPa
6240 psi
ASTM D412
Tensile Strength, Yield 22.0 MPa

@Strain 100 %
3190 psi

@Strain 100 %
ASTM D-412
36.0 MPa

@Strain 300 %
5220 psi

@Strain 300 %
ASTM D-412
Elongation at Break 450 %
450 %
ASTM D412
Tear Strength 195 kN/m
1110 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 50
50
H-18 wheel; ASTM D-1044.
Tensile Set 110 %
110 %
at break; ASTM D-412