Mechanical Properties Metric English Comments
Tensile Strength, Yield 317 MPa

@Thickness 3.17 mm
46000 psi

@Thickness 0.125 in
LW
Industrial Laminates/Norplex MC514MG Glass Fabric
Description: MC514MG is made with a woven glass fabric in combination with high temperature, conductive, phenolic resin system.NP514MG has excellent flexural, compressive and impact strengths at roo..
Tensile Strength, Yield 317 MPa

@Temperature 204 °C
46000 psi

@Temperature 400 °F
Special Metals INCOLOY® 25-6HN Super-Austenitic Stainless Steel
INCOLOY alloy 25-6HN is a super-austenitic stainless steel containing 6% molybdenum and with properties enhanced by its content of nitrogen. Its high content of nickel results in thermal stability ..
Tensile Strength, Yield 317 MPa

@Temperature 260 °C
46000 psi

@Temperature 500 °F
Special Metals INCOLOY® 25-6HN Super-Austenitic Stainless Steel
INCOLOY alloy 25-6HN is a super-austenitic stainless steel containing 6% molybdenum and with properties enhanced by its content of nitrogen. Its high content of nickel results in thermal stability ..
Tensile Strength, Yield >= 317 MPa

@Strain 0.200 %,
Thickness 7.90 - 50.8 mm
>= 46000 psi

@Strain 0.200 %,
Thickness 0.311 - 2.00 in
Tempers T851/T852
Constellium Alumold® 350 Aluminum
Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti..
Tensile Strength, Yield 317 MPa

@Temperature 649 °C
46000 psi

@Temperature 1200 °F
Tempering Temperature-1200°F
Crucible Steel 422 Stainless Steel
Crucible 422 is a hardenable martensitic stainless steel which is being widely used for high temperatures up to 1200°F. It has excellent creep-rupture properties in the range of 600/1200°F and is..