Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 290 MPa @Strain 0.200 % |
42100 psi @Strain 0.200 % |
Outokumpu Typical,Cold Rolled Strip/Sheet; EN 10002-1 |
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Yield | 290 MPa @Strain 1.00 %, Temperature -80.0 °C |
42100 psi @Strain 1.00 %, Temperature -112 °F |
EN min.; EN 10002-5 |
Outokumpu 4307 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Yield | 290 MPa @Strain 1.00 % |
42100 psi @Strain 1.00 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto), hot rolled strip/sheet (C.. |
|||
Tensile Strength, Yield | 290 MPa @Strain 1.00 % |
42100 psi @Strain 1.00 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4550 Austenitic Stainless Steel Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto) and rod forms. |
|||
Tensile Strength, Yield | 290 MPa @Strain 1.00 % |
42100 psi @Strain 1.00 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4878 High Temperature Austenitic Stainless Steel Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For .. |
|||
Tensile Strength, Yield | 290 MPa @Temperature 71.1 °C |
42000 psi @Temperature 160 °F |
0° Direction, Wet; ASTM D638 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Tensile Strength, Yield | 290 MPa @Temperature 71.1 °C |
42000 psi @Temperature 160 °F |
0° Direction, Dry; Autoclave, 50 psi, 90min; ASTM D638 |
Park Electrochemical Nelcote® F-529 Phenolic Prepreg, 7781 E-Glass Reinforced Nelcote® F-529 is a non-halogenated phenolic resin designed specifically for use in aircraft and mass-transit interior laminate and sandwich panels. F-529 was formulated for applications requiring .. |
|||
Tensile Strength, Yield | 290 MPa @Thickness 3.17 mm |
42000 psi @Thickness 0.125 in |
LW |
Industrial Laminates/Norplex NP841 Glass Fabric
(discontinued **) Description: Woven glass fabric with phenolic resin. Contains Kocite® for controlled conductivity. Acts as static electricity drain to protect electrical and electronic equipment.Thickness Tested: .. |
|||
Tensile Strength, Yield | 290 MPa @Thickness 1.57 mm |
42000 psi @Thickness 0.0620 in |
LW; ASTM D638 |
Industrial Laminates/Norplex NP504 Glass Fabric Description: Woven glass fabric with high temperature phenolic resin. Good flexural, compressive and impact strengths at elevated temperatures. Capable of continuous operation at 175° C, see note.. |
|||
Tensile Strength, Yield | >= 290 MPa @Strain 0.200 % |
>= 42100 psi @Strain 0.200 % |
|
Industeel CLC 18.12.4 LN 3%Mo Austenitic Stainless Steel with Nitrogen Addition Description: CLC 18-12-4LN (317LN) is a Nitrogen alloyed austenitic stainless steel with a 3% Mo minimum addition (>4%). Alloys CLC 18-12-4LN (317LN) exhibit austenitic microstructure free of delete.. |
|||
Tensile Strength, Yield | >= 290 MPa @Strain 0.200 %, Thickness 127 - 152.4 mm |
>= 42100 psi @Strain 0.200 %, Thickness 5.00 - 6.000 in |
Tempers T851/T852 |
Constellium Alumold® 350 Aluminum Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti.. |
|||
Tensile Strength, Yield | 290 MPa @Strain 0.200 % |
42100 psi @Strain 0.200 % |
ASTM E8 |
ATI Allegheny Ludlum 309 Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Tensile Strength, Yield | 290 MPa @Strain 0.200 % |
42100 psi @Strain 0.200 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4948 High Temperature Austenitic Stainless Steel Creep-resistant variant of 1.4301, with a standardized minimum carbon content for service at temperatures of up to 800°C in dry air.Applications: Heat and creep resistance. For use over 550°C for.. |
|||
Tensile Strength, Yield | 290 MPa @Strain 0.200 % |
42100 psi @Strain 0.200 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 725LN Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form. |
|||
Tensile Strength, Yield | 290 MPa @Strain 1.00 % |
42100 psi @Strain 1.00 % |
Typical after Solution Annealing |
Industeel UREA 25.22.2 Plants Description: CLI UREA 25.22.2 chemical composition has been optimized for specific uses in Urea plants. It is a 310L modified austenitic stainless steel with low carbon, low silicon and high nitroge.. |