Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 276 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 276 MPa

@Thickness 1.57 mm
40000 psi

@Thickness 0.0620 in
LW; ASTM D638
Industrial Laminates/Norplex NP510A Glass Fabric
Description: Woven glass fabric epoxy laminate. Engineered to provide NEMA grade FR-4 properties. This material contains bromine on the epoxy resin backbone. Certifiable to MIL-I-24768/27, Type GEE-..
Tensile Strength, Yield 276 MPa

@Thickness 3.17 mm
40000 psi

@Thickness 0.125 in
CW
Industrial Laminates/Norplex P95 Glass Fabric
Description: Woven glass fabric with polyimide resin engineered to maintain excellent physical properties at 240°C. Low coefficient of thermal expansion, high mechanical strength.Thickness Tested..
Tensile Strength, Yield 276 MPa

@Thickness 3.17 mm,
Temperature 538 °C
40000 psi

@Thickness 0.125 in,
Temperature 1000 °F
0.2% offset
Haynes Hastelloy® C-22® alloy, transverse, GTAW weldment, sheet - plate
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Tensile Strength, Yield 276 MPa

@Thickness 3.20 mm,
Temperature 371 °C
40000 psi

@Thickness 0.126 in,
Temperature 700 °F
0.2% Offset
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Sheet, Cold Rolled and Solution Annealed
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Tensile Strength, Yield 276 MPa

@Temperature 427 °C
40000 psi

@Temperature 800 °F
Special Metals INCOLOY® 25-6HN Super-Austenitic Stainless Steel
INCOLOY alloy 25-6HN is a super-austenitic stainless steel containing 6% molybdenum and with properties enhanced by its content of nitrogen. Its high content of nickel results in thermal stability ..
Tensile Strength, Yield 276 MPa

@Strain 0.200 %
40000 psi

@Strain 0.200 %
Annealed Sheet, 0.15-1.6mm thick
Special Metals INCOLOY® alloy 864
INCOLOY® alloy 8684 (UNS S35135) was specifically developed for automotive exhaust system flexible couplings, EGR tubes, manifolds and tailpipes. It exhibits excellent fatigue resistance, therma..
Tensile Strength, Yield 276 MPa

@Strain 0.200 %
40000 psi

@Strain 0.200 %
as rolled
Carlson C 400 Nickel-Copper Alloy
General DescriptionCarlson Alloy C 400 is a nickel-copper alloy which provides an excellent combination of high strength, ductility, good weldability, and resistance to corrosion over a wide range o..
Tensile Strength, Yield 276 MPa

@Strain 0.200 %
40000 psi

@Strain 0.200 %
Annealed
AK Steel 301 Austenitic Stainless steel
AK Steel 301 provides high strength and good ductility when cold worked. It is a modification of AK Steel 302 to increase the cold work-hardening range, to permit higher tensile strengths to be ach..
Tensile Strength, Yield 276 MPa

@Strain 0.200 %
40000 psi

@Strain 0.200 %
Annealed
AK Steel 420 Martensitic Stainless steel
AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu..
Tensile Strength, Yield 276 MPa

@Strain 0.200 %
40000 psi

@Strain 0.200 %
Annealed
AK Steel 420 ULTRA HONE® Martensitic Stainless steel
AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu..
Tensile Strength, Yield 276 MPa

@Strain 0.200 %
40000 psi

@Strain 0.200 %
Annealed
AK Steel 420HC Martensitic Stainless steel
AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu..
Tensile Strength, Yield 276 MPa

@Strain 0.200 %
40000 psi

@Strain 0.200 %
Annealed
AK Steel 420LC Martensitic Stainless steel
AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu..
Tensile Strength, Yield 276 MPa

@Strain 0.200 %,
Thickness 1.02 - 38.1 mm
40000 psi

@Strain 0.200 %,
Thickness 0.0400 - 1.50 in
Rolled Plate
Magnesium Elektron Elektron® 43 Magnesium Wrought Alloy
High strength wrought Mg alloy available as rolled plate, forging feedstock, and extrusions. It is a wrought evolution of the casting alloy Elektron WE43. Elektron 43 uses zirconium grain refining..