Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 27.0 MPa @Temperature 1093 °C |
3920 psi @Temperature 1999 °F |
ASTM E8 |
ATI Allegheny Ludlum 310S Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Tensile Strength, Yield | 27.0 MPa @Strain 100 % |
3920 psi @Strain 100 % |
ASTM D-412 |
BASF Elastollan® S64D Polyester Type Polyurethane Elastomer Recommended for injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fuel and solv.. |