Mechanical Properties Metric English Comments
Tensile Strength, Yield 1310 MPa

@Strain 0.200 %
190000 psi

@Strain 0.200 %
48 HRC
Schmolz + Bickenbach Thermodur® 2344 Magnum Hot Work Die Steel
Description: Thermodur® 2344 Magnum is an electro slag remelted (ESR) hot work die steel, designed to meet all die casting industry specificationCharacteristics: Excellent toughness; Excellent re..
Tensile Strength, Yield >= 1310 MPa

@Strain 0.200 %
>= 190000 psi

@Strain 0.200 %
PSM Industries PolyAlloys MIM-4605 quench/temper Low Alloy Steel
PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl..