Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 19.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.0 MPa

@Strain 10.0 %
2760 psi

@Strain 10.0 %
ISO 527-1/-2
DSM Arnitel® UM622 General Purpose Grade Copolyester Elastomer (North America)  (discontinued **)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 19.0 MPa

@Strain 10.0 %
2760 psi

@Strain 10.0 %
ISO 527-1/-2
DSM Arnitel® UM622 Polyether Ester Elastomer (European Grade)  (discontinued **)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 19.0 MPa

@Strain 100 %
2760 psi

@Strain 100 %
ASTM D412
GRECO ISOTHANE 1055D Poly(adipate)ester TPU Resin
ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products ..
Tensile Strength, Yield 19.0 MPa

@Strain 100 %
2760 psi

@Strain 100 %
ASTM D412
GRECO ISOTHANE 3065D Polyether TPU Resin
ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod..
Tensile Strength, Yield 19.0 MPa

@Strain 50.0 %
2760 psi

@Strain 50.0 %
ASTM D412
GRECO ISOTHANE 1065D Poly(adipate)ester TPU Resin
ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products ..
Tensile Strength, Yield 19.0 MPa

@Strain 100 %
2760 psi

@Strain 100 %
ASTM D412
GRECO ISOTHANE 1160D Poly(adipate)ester TPU Resin
ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp..
Tensile Strength, Yield 19.0 MPa

@Temperature 23.0 °C
2760 psi

@Temperature 73.4 °F
90°
Hexcel® HexPly® 954-6 Curing Cyanate Resin, K13C-2U Fiber
Information provided by HexCel
Tensile Strength, Yield 19.0 MPa

@Strain 100 %
2760 psi

@Strain 100 %
ASTM D-412
BASF Elastollan® S98A Polyester Type Polyurethane Elastomer
Recommended for injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fuel and solv..
Tensile Strength, Yield 19.0 MPa

@Strain 300 %
2760 psi

@Strain 300 %
0.76 mm (0.030 in) extruded sheet; ASTM D-412
BASF Elastollan® 1185A10X Wire & Cable Grade Polyurethane Elastomer
Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.
Tensile Strength, Yield 19.0 MPa

@Strain 300 %
2760 psi

@Strain 300 %
0.76 mm (0.030 in) extruded sheet; ASTM D-412
BASF Elastollan® 1185A10U Wire & Cable Grade Polyurethane Elastomer
As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.
Tensile Strength, Yield 19.0 MPa

@Strain 300 %
2760 psi

@Strain 300 %
0.76 mm (0.030 in) extruded sheet; ASTM D-412
BASF Elastollan® 1185A10V Wire & Cable Grade Polyurethane Elastomer
Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.