Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 124 MPa @Strain 0.200 % |
18000 psi @Strain 0.200 % |
|
PSM Industries PolyAlloys MIM-2200 sintered Low Alloy Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Tensile Strength, Yield | 124 MPa @Thickness 1.57 mm |
18000 psi @Thickness 0.0620 in |
LW; ASTM D638 |
Industrial Laminates/Norplex NP611 Paper Base Laminate Description: Hot punching general-purpose phenolic grade. Mechanical properties approach those of NP610 with improved electrical properties and moisture resistance.Thickness Tested: 0.062", 0 125" a.. |
|||
Tensile Strength, Yield | 124 MPa @Strain 0.200 %, Temperature 300 °C |
18000 psi @Strain 0.200 %, Temperature 572 °F |
|
Magnesium Elektron Elektron® 675 Magnesium Wrought Alloy High strength wrought Mg alloy used for high performance components, including at elevated temperature. Excellent corrosion resistance and easily machined. Can be extruded, forged and hot formed. .. |
|||
Tensile Strength, Yield | 124 MPa @Strain 0.200 %, Thickness >=63.5 mm |
18000 psi @Strain 0.200 %, Thickness >=2.50 in |
|
Carlson 70 30 Cu Ni Copper-Nickel Alloy General DescriptionCarlson alloy 70 30 Cu Ni is a copper nickel alloy with excellent resistance to corrosion and erosion. It is strong and ductile. 70 30 Cu Ni is utilized in areas where high temp.. |
|||
Tensile Strength, Yield | 124 MPa @Strain 0.200 %, Temperature 871 °C |
18000 psi @Strain 0.200 %, Temperature 1600 °F |
Solution Annealed Tubing |
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar.. |