Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1210 MPa @Temperature 427 °C |
175000 psi @Temperature 800 °F |
|
QuesTek® Innovations Ferrium® C61™ Case-hardened Gear Steel with Ultrahigh-strength Core Description: Ferrium® C61™ is a member of a new class of martensitic secondary-hardening gear and bearing steels that utilize an efficient M2C precipitate strengthening dispersion. Because of the .. |
|||
Tensile Strength, Yield | 1210 MPa @Temperature 392 °C |
175000 psi @Temperature 738 °F |
|
Schmolz + Bickenbach Thermodur® 2714 Extra Fine Structure - Hot Work Die Steel Description: Thermodur 2714 is an Extra Fine Structure (EFS) nickel based tool steel.Characteristics: Excellent high temperature strength; Good toughness; and Good resistance to thermal shockApplica.. |
|||
Tensile Strength, Yield | 1210 MPa @Strain 0.200 % |
175000 psi @Strain 0.200 % |
hardness of 44 HRC |
Bohler-Uddeholm UDDEHOLM DIEVAR® Hot Work Tool Steel Description: Uddeholm Dievar is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross cracking, hot wear and plastic.. |
|||
Tensile Strength, Yield | 1210 MPa @Strain 0.200 % |
175000 psi @Strain 0.200 % |
42 HRC |
Schmolz + Bickenbach Formadur® PH X Superclean Plastic Mold Steel Description: Formadur® PH X Superclean is a corrosion-resistant, martensitic precipitation hardened stainless steelCharacteristics: Excellent resistance to corrosion; Excellent polishability; Excel.. |