Polymer Property : Tensile Strength, Yield = 1640 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 11.3 MPa

@Strain 10.0 %
1640 psi

@Strain 10.0 %
ISO 527-1/-2
DSM Arnitel® PL471 45 Shore D, Injection Grade Copolyester Elastomer (North America)  (discontinued **)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 11.3 MPa

@Strain 10.0 %
1640 psi

@Strain 10.0 %
ASTM D638
SK Chemicals SKYPEL M555DH General Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Tensile Strength, Yield 11.3 MPa

@Strain 10.0 %
1640 psi

@Strain 10.0 %
ASTM D638
SK Chemicals SKYPEL G455D Special Grade Oil-Resistant Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Tensile Strength, Yield 11.3 MPa

@Strain 5.00 %
1640 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® PB582-H 58 Shore D, Blow Molding Grade, Heat Stabilized Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 11.3 MPa

@Strain 5.00 %
1640 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® PB582-H Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 11.3 MPa

@Strain 50.0 %
1640 psi

@Strain 50.0 %
ISO 527-1/-2
DSM Arnitel® EB464 42 Shore D, Blow Molding Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 11.3 MPa

@Strain 50.0 %
1640 psi

@Strain 50.0 %
ISO 527-1/-2
DSM Arnitel® EB464 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 11.3 MPa

@Strain 10.0 %
1640 psi

@Strain 10.0 %
ISO 527-1/-2
DSM Arnitel® PL471 Polyether Ester Elastomer (European Grade)  (discontinued **)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..