Mechanical Properties Metric English Comments
Tensile Strength, Yield 909.76 MPa

@Strain 0.200 %
131950 psi

@Strain 0.200 %
after porcelain firing
Wieland Simidur S 2 PFM Alloy
Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental